Polymer Property : Fracture Toughness = 77.0 ksi-in½ Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Fracture Toughness 60.0 - 84.6 MPa-m½
54.6 - 77.0 ksi-in½
ATI Wah Chang 425™ Titanium Alloy, Hot Rolled & Annealed Plate
ATI 425™ titanium is an innovative high strength alloy that has strength comparable to Ti-6-4, yet has the advantage that it can be cold worked. Originally developed for armor plate for ballistic p..