Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Fracture Toughness | >= 60.0 MPa-m½ | >= 54.6 ksi-in½ | ST then Aged 8 hrs |
TIMET 10-2-3 Titanium Alloy (Ti-10V-2Fe-3Al), Aged Billet/Bar per ASTM 4986 High-Strength Forging Alloy.Industry Specifications: USA Aerospace: AMS 4986.Features: A readily forgeable alloy that offers excellent combinations of strength, ductility, fracture toughness and hi.. |
|||
Fracture Toughness | 60.0 - 84.6 MPa-m½ | 54.6 - 77.0 ksi-in½ | |
ATI Wah Chang 425™ Titanium Alloy, Hot Rolled & Annealed Plate ATI 425™ titanium is an innovative high strength alloy that has strength comparable to Ti-6-4, yet has the advantage that it can be cold worked. Originally developed for armor plate for ballistic p.. |