Mechanical Properties Metric English Comments
Fracture Toughness >= 66.0 MPa-m½
>= 60.1 ksi-in½
Latrobe Marvac 300 VIM-VAR ; 10 in. High Strength Maraging Steel
MARVAC 300 VIM-VAR is a low carbon maraging steel capable of 270,000 psi minimum yield strength, coupled with excellent toughness and ductility. The alloy has good fabrication characteristics, which..
Fracture Toughness >= 66.0 MPa-m½
>= 60.1 ksi-in½
Latrobe Marvac 300 VIM-VAR ; 6.25 in. High Strength Maraging Steel
MARVAC 300 VIM-VAR is a low carbon maraging steel capable of 270,000 psi minimum yield strength, coupled with excellent toughness and ductility. The alloy has good fabrication characteristics, which..
Fracture Toughness >= 66.0 MPa-m½
>= 60.1 ksi-in½
Latrobe Marvac 300 VIM-VAR ; 5 RCS High Strength Maraging Steel
MARVAC 300 VIM-VAR is a low carbon maraging steel capable of 270,000 psi minimum yield strength, coupled with excellent toughness and ductility. The alloy has good fabrication characteristics, which..