Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Fracture Toughness | >= 66.0 MPa-m½ | >= 60.1 ksi-in½ | |
Latrobe Marvac 300 VIM-VAR ; 10 in. High Strength Maraging Steel MARVAC 300 VIM-VAR is a low carbon maraging steel capable of 270,000 psi minimum yield strength, coupled with excellent toughness and ductility. The alloy has good fabrication characteristics, which.. |
|||
Fracture Toughness | >= 66.0 MPa-m½ | >= 60.1 ksi-in½ | |
Latrobe Marvac 300 VIM-VAR ; 6.25 in. High Strength Maraging Steel MARVAC 300 VIM-VAR is a low carbon maraging steel capable of 270,000 psi minimum yield strength, coupled with excellent toughness and ductility. The alloy has good fabrication characteristics, which.. |
|||
Fracture Toughness | >= 66.0 MPa-m½ | >= 60.1 ksi-in½ | |
Latrobe Marvac 300 VIM-VAR ; 5 RCS High Strength Maraging Steel MARVAC 300 VIM-VAR is a low carbon maraging steel capable of 270,000 psi minimum yield strength, coupled with excellent toughness and ductility. The alloy has good fabrication characteristics, which.. |