Polymer Property : Fracture Toughness = 6.55 ksi-in½
Polymer Property :
Fracture Toughness =
6.55 ksi-in½
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Fracture Toughness
7.20
MPa-m½
6.55
ksi-in½
CeramTec 965 Toughened Alumina (Al2O3-ZrO2)
Hasselman Thermal Shock value is 270 K.Data provided by CeramTec North America.