Polymer Property : Fracture Toughness = 6.37 ksi-in½ Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Fracture Toughness 7.00 MPa-m½
6.37 ksi-in½
K<sub>IC</sub> (SEVNB); DIN CEN/TS 14425-1
CeramTec SL 200 BG Silicon Nitride, Si3N4-Y2O3
SL 200 BG is a silicon nitride ceramic used to make welding rollers, pins, and components, gas nozzles, and forming tools. Silicon nitrides are ideal for components working under mechanical loads an..
Fracture Toughness 7.00 MPa-m½
6.37 ksi-in½
DIN 51109
CeramTec SL 200 ST Silicon Nitride, Si3N4-Y2O3
SL 200 ST is a silicon nitride ceramic especially suitable for components exposed to mechanical stress and engine-specific applications even at elevated temperatures. It is recognized for its high s..
Fracture Toughness 7.00 MPa-m½
6.37 ksi-in½
Wieland Zeno™ Zr Disc Zirconium Oxide
Zirconium oxide blanks supplied partly sintered. Available in five different thicknesses to reduce material costs. Applications: modern dental restorationsDental
Fracture Toughness 7.00 MPa-m½
6.37 ksi-in½
Astro Met AmZirOx 86 Zirconia - Zirconium Oxide
General Description:AmZirOx 86 zirconia (Astro Met Zirconium Oxide) is a yttria stabilized zirconia ceramic material which features high strength and toughness making it a candidate material for use..
Fracture Toughness 7.00 MPa-m½
6.37 ksi-in½
Ceradyne Ekatherm EKasin® S Gas Pressure Sintered Silicon Nitride (Si3N4)
EKatherm® Silicon Nitride is the state-of-the-art material for a wide variety of components used in Aluminum Alloy casting processes.Features: High Temperature Resistance High Thermal Shock Resist..