Material Notes:
Zirconium oxide blanks supplied partly sintered. Available in five different thicknesses to reduce material costs. Applications: modern dental restorationsDental
Physical Properties Metric English Comments
Density >= 6.06 g/cc
>= 0.219 lb/in³
Open Porosity 0.00 %
0.00 %
Mechanical Properties Metric English Comments
Hardness, Vickers <= 1290
<= 1290
Modulus of Elasticity 210 GPa
30500 ksi
Flexural Strength <= 1300 MPa
<= 189000 psi
4-point
Compressive Strength 2000 MPa
290000 psi
Fracture Toughness 7.00 MPa-m½
6.37 ksi-in½
Thermal Properties Metric English Comments
CTE, linear 10.0 µm/m-°C

@Temperature 25.0 - 500 °C
5.56 µin/in-°F

@Temperature 77.0 - 932 °F
Component Elements Properties Metric English Comments
Al2O3 <= 1.0 %
<= 1.0 %
Y2O3 4.0 %
4.0 %
ZrO2 95 %
95 %
Descriptive Properties Value Comments
Color white / x-ray opaque