Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Fracture Toughness | 6.00 MPa-m½ | 5.46 ksi-in½ | |
Osprey Metals CE7 Al-Si Controlled Expansion Alloy Si-30%Al controlled expansion alloy manufactured and patented by Osprey Metals Ltd.Information provided to MatWeb by Osprey Metals. |
|||
Fracture Toughness | 6.00 - 6.80 MPa-m½ | 5.46 - 6.19 ksi-in½ | |
China-Yixing Longly Refractories Alumina Plates and Pieces Microcrystal Wear-Resistant Alumina Ceramic Lining Plates and Pieces LONGLY's wear-resistant alumina ceramic lining plates and pieces are special alumina ceramics produced on the basis of Al2O3 by dry pressing with rare metal oxide as solvent, sintered under a high t.. |
|||
Fracture Toughness | 6.00 MPa-m½ | 5.46 ksi-in½ | |
Astro Met ZTA 96 Zirconia Toughened Alumina General Description:ZTA-96 is a zirconia toughened alumina ceramic that exhibits excellent wear and corrosion resistance along with high strength and toughness. Astro Met has developed ZTA-96 zircon.. |
|||
Fracture Toughness | 6.00 MPa-m½ | 5.46 ksi-in½ | |
Ceradyne Ceralloy® 147-31E Sintered Reaction Bonded Silicon Nitride (Si3N4) Ceralloy® 147 Reaction Bonded Silicon Nitride (RBSN) is a high purity grade of silicon nitride. RBSN has excellent thermal shock resistance and outstanding compatibility with non-ferrous molten met.. |
|||
Fracture Toughness | 6.00 MPa-m½ | 5.46 ksi-in½ | |
Ceradyne Ceralloy® 147-5 Silicon Nitride Ceralloy® 147 Hot Pressed Silicon Nitride (HPSN) can be formulated into a variety of compositions having minimal densification aids. These HPSN compositions offer the highest strength of Ceradyne's.. |
|||
Fracture Toughness | 6.00 MPa-m½ | 5.46 ksi-in½ | DIN 51109 |
CeramTec 950 Zirconia Toughened Alumina (ZTA), Al2O3•ZrO2 950 has a combination of high strength (from zirconia) and high hardness (from the alumina phase). It has excellent wear resistance, both in sliding and abrasive conditions. This material offers a g.. |
|||
Fracture Toughness | 6.00 MPa-m½ | 5.46 ksi-in½ | |
Ceradyne Ceralloy® 147-31N Sintered Reaction Bonded Silicon Nitride (Si3N4) Ceralloy® 147 Reaction Bonded Silicon Nitride (RBSN) is a high purity grade of silicon nitride. RBSN has excellent thermal shock resistance and outstanding compatibility with non-ferrous molten met.. |