Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Fracture Toughness | 4.80 MPa-m½ | 4.37 ksi-in½ | ASTM C1421 |
M Cubed Technologies TSC-15 Titanium-alloyed Reaction Bonded Silicon Carbide Specialty reaction-bonded SiC for applications requiring high stiffness, high toughness, and also high thermal conductivity--mechanical seals, for example Flow-through complex channels can be forme.. |