Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Fracture Toughness | 3.20 MPa-m½ | 2.91 ksi-in½ | DIN 51109 |
CeramTec 192/193 Titania 192/193 is an excellent material for textile and other structural applications, where superior surface finishes are required with high chemical resistance. 193 is identical except it is metallic gra.. |
|||
Fracture Toughness | 3.20 MPa-m½ | 2.91 ksi-in½ | Notched Beam |