Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Fracture Toughness | 3.10 MPa-m½ | 2.82 ksi-in½ | |
Ceradyne CeraTrex™ SC-P2 Silicon Carbide Features:purity>99.9995%corrosion resistancewear resistancenear net shape fabrication to 400 mm OD Applications:semiconductor componentswear componentsInformation provided by Ceradyne Company |
|||
Fracture Toughness | 3.10 MPa-m½ | 2.82 ksi-in½ | |
Ceradyne CeraTrex™ SC-P3 Silicon Carbide Features:purity>99.9995%corrosion resistancewear resistancenear net shape fabrication to 400 mm OD Applications:semiconductor componentswear componentsInformation provided by Ceradyne Company |