Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Fracture Toughness | 15.0 - 30.0 MPa-m½ | 13.7 - 27.3 ksi-in½ | |
MMCC Al/Al2O3 3DP Particulate Aluminum Matrix Composite Cast, discontinuously reinforced aluminum matrix composite. May be fabricated by vacuum infiltration of the ceramic preform.Data provided by the manufacturer, Metal Matrix Cast Composites (MMCC). |
|||
Fracture Toughness | 15.0 - 30.0 MPa-m½ | 13.7 - 27.3 ksi-in½ | |
MMCC Al/Al2O3 Particulate Aluminum Matrix Composite Cast, discontinuously reinforced aluminum matrix composite. May be fabricated by vacuum infiltration of the ceramic preform.Data provided by the manufacturer, Metal Matrix Cast Composites (MMCC). |