Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Fracture Toughness | 15.0 - 30.0 MPa-m½ | 13.7 - 27.3 ksi-in½ | |
MMCC Al/Al2O3 3DP Particulate Aluminum Matrix Composite Cast, discontinuously reinforced aluminum matrix composite. May be fabricated by vacuum infiltration of the ceramic preform.Data provided by the manufacturer, Metal Matrix Cast Composites (MMCC). |
|||
Fracture Toughness | 15.0 - 30.0 MPa-m½ | 13.7 - 27.3 ksi-in½ | |
MMCC Al/Al2O3 Particulate Aluminum Matrix Composite Cast, discontinuously reinforced aluminum matrix composite. May be fabricated by vacuum infiltration of the ceramic preform.Data provided by the manufacturer, Metal Matrix Cast Composites (MMCC). |
|||
Fracture Toughness | 15.0 - 20.0 MPa-m½ | 13.7 - 18.2 ksi-in½ | |
MMCC Al/Al2O3 Short Fiber Aluminum Matrix Composite Cast, discontinuously reinforced aluminum matrix composite. May be fabricated by vacuum infiltration of the ceramic preform.Data provided by the manufacturer, Metal Matrix Cast Composites (MMCC). |
|||
Fracture Toughness | 15.0 - 25.0 MPa-m½ | 13.7 - 22.8 ksi-in½ | |
MMCC Al/SiC 3DP Particulate Aluminum Matrix Composite Cast, discontinuously reinforced aluminum matrix composite. May be fabricated by vacuum infiltration of the ceramic preform.Data provided by the manufacturer, Metal Matrix Cast Composites (MMCC). |
|||
Fracture Toughness | 15.0 MPa-m½ | 13.7 ksi-in½ | ASTM C1421 |
M Cubed Technologies ASC-301 Aluminum alloy-30% SiC Metal Matrix Composite High stiffness, low density composite. Parts are cast using several standard foundry techniques Size range varies from small components (1lb or smaller) to parts greater than 10 ft. square with co.. |