Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Fracture Toughness | 23.9 MPa-m½ | 21.8 ksi-in½ | Average value K<sub>IC</sub> LT orientation. |
Materion AlBeMet® AM 162 Extruded Bar, Annealed Mechanical property values below are in the longitudinal direction; transverse values generally lower. This is a powder metallurgical product produced by gas atomization available as rod, bar, tube.. |