Polymer Property : Fracture Toughness = 21.8 ksi-in½ Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Fracture Toughness 23.9 MPa-m½
21.8 ksi-in½
Average value K<sub>IC</sub> LT orientation.
Materion AlBeMet® AM 162 Extruded Bar, Annealed
Mechanical property values below are in the longitudinal direction; transverse values generally lower. This is a powder metallurgical product produced by gas atomization available as rod, bar, tube..