Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Fracture Toughness | 11.3 MPa-m½ | 10.3 ksi-in½ | |
Ceramic Process Systems AlSiC-9, 63 vol% SiC Aluminum alloy A356.2 used. Hermeticity < 1x109 atm-cc/s He.CPS fabricates AlSiC by preparing an SiC preform which is subsequently infiltrated by molten aluminum metal. After infiltration, compone.. |
|||
Fracture Toughness | 11.3 MPa-m½ | 10.3 ksi-in½ | Average value K<sub>IC</sub> TL orientation. |
Materion AlBeMet® AM 162 Extruded Bar, Annealed Mechanical property values below are in the longitudinal direction; transverse values generally lower. This is a powder metallurgical product produced by gas atomization available as rod, bar, tube.. |