Polymer Property : Fracture Toughness = 10.3 ksi-in½ Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Fracture Toughness 11.3 MPa-m½
10.3 ksi-in½
Ceramic Process Systems AlSiC-9, 63 vol% SiC
Aluminum alloy A356.2 used. Hermeticity < 1x109 atm-cc/s He.CPS fabricates AlSiC by preparing an SiC preform which is subsequently infiltrated by molten aluminum metal. After infiltration, compone..
Fracture Toughness 11.3 MPa-m½
10.3 ksi-in½
Average value K<sub>IC</sub> TL orientation.
Materion AlBeMet® AM 162 Extruded Bar, Annealed
Mechanical property values below are in the longitudinal direction; transverse values generally lower. This is a powder metallurgical product produced by gas atomization available as rod, bar, tube..