Polymer Property : Fracture Toughness = 0.900 MPa-m½ Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Fracture Toughness 0.900 MPa-m½
0.819 ksi-in½
Hexcel® HexPly® M36 180°C (350°F) Curing Epoxy Matrix
HexPly® M36 is a high performance 180ºC cure matrix developed for aerospace and industrial markets. It can be used in a variety of production techniques (Resin Film Infusion (RFI), prepreg and sem..