Polymer Property : Fracture Toughness = 0.660 MPa-m½ Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Fracture Toughness 0.660 MPa-m½
0.601 ksi-in½
Corning Antimicrobial Gorilla® Glass Touch Screen Glass
Antimicrobial Corning® Gorilla® Glass is an antimicrobial cover glass with EPA registration as a treated article. It combines the benefits of Corning® Gorilla® Glass technology, including durabi..
Fracture Toughness 0.660 MPa-m½
0.601 ksi-in½
Corning Gorilla® Glass 3 Touch Screen Glass with NDR
Gorilla® Glass 3 with Native Damage Resistance™ (NDR) is an alkali-aluminosilicate thin sheet glass that is better able to survive the real-world events that most commonly cause glass failure. Wit..