Fracture Toughness 0.639 MPa-m½
0.582 ksi-in½
Hexcel® HexPly® F652 Bismaleimide Resin
HexPly® F652 is a bismaleimide resin that cures via an addition reaction with no condensation by-products. HexPly® F652 is a controlled flow polyimide resin system designed for alternative process..