Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Fracture Toughness | 0.639 MPa-m½ | 0.582 ksi-in½ | |
Hexcel® HexPly® F652 Bismaleimide Resin HexPly® F652 is a bismaleimide resin that cures via an addition reaction with no condensation by-products. HexPly® F652 is a controlled flow polyimide resin system designed for alternative process.. |