Tensile Modulus 6.67 GPa
967 ksi
ASTM D882
UBE UPISEL-N BE1210 Copper Clad Laminate
Description: UPISEL-N BE1210 is non-adhesive type flexible Copper Clad Laminate (Polyimide = 25µm, Cu = 18µm) based on "UPILEX-VT." UPISEL-N has excellent dimensional stability and heat resistance..