Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 6.67 GPa | 967 ksi | ASTM D882 |
UBE UPISEL-N BE1210 Copper Clad Laminate Description: UPISEL-N BE1210 is non-adhesive type flexible Copper Clad Laminate (Polyimide = 25µm, Cu = 18µm) based on "UPILEX-VT." UPISEL-N has excellent dimensional stability and heat resistance.. |