Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.665 GPa | 96.5 ksi | 100 micron film; ASTM D882 |
Kaneka PHBH Semi-Rigid Bio-based Polymer A copolymer produced of 3-hydroxybutyrate and 3-hydroxyhexanoate produced by fermentation of plant oils. It has excellent biodegradability (under anaerobic, aerobic, aquatic, and compost conditions.. |