Mechanical Properties Metric English Comments
Tensile Modulus 0.665 GPa
96.5 ksi
100 micron film; ASTM D882
Kaneka PHBH Semi-Rigid Bio-based Polymer
A copolymer produced of 3-hydroxybutyrate and 3-hydroxyhexanoate produced by fermentation of plant oils. It has excellent biodegradability (under anaerobic, aerobic, aquatic, and compost conditions..