Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.660 GPa | 95.7 ksi | MD; ASTM D882 |
Honeywell Aegisâ„¢ H135ZP Nylon 6 Extrusion Grade Homopolymer Film Description: Aegis H135ZP is a high viscosity, nylon 6 film extrusion grade homopolymer for cast or blown film. It conforms to Food and Drugs Administration requirements of 21 CFR 177.1500 for nylon.. |
|||
Tensile Modulus | 0.660 GPa | 95.7 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Stat-kon FX97333 PE LNP* Stat-kon* FX97333 is a compound based on Polyethylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for th.. |
|||
Tensile Modulus | 0.660 GPa | 95.7 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Stat-kon FX97333 PE (Asia Pacific) LNP* Stat-kon* FX97333 is a compound based on Polyethylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for th.. |