Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.640 GPa | 92.8 ksi | MD; ASTM D882 |
Honeywell Aegisâ„¢ H135MP Nylon 6 Extrusion Grade Homopolymer Film Description: Aegis H135MP is a lubricated and nucleated high viscosity, nylon 6 extrusion grade homopolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21 CFR.. |
|||
Tensile Modulus | 0.640 GPa | 92.8 ksi | TD; ASTM D882 |
Honeywell Aegisâ„¢ H135ZP Nylon 6 Extrusion Grade Homopolymer Film Description: Aegis H135ZP is a high viscosity, nylon 6 film extrusion grade homopolymer for cast or blown film. It conforms to Food and Drugs Administration requirements of 21 CFR 177.1500 for nylon.. |
|||
Tensile Modulus | 0.640 GPa | 92.8 ksi | 1 mm/min |
Arkema Group Rilsan® MA 4420 Nylon 12, Flexible Tubing Grade (Conditioned) Designation ISO 1874-PA12-HI,EHL,22-003Flexible grade for tubes extrusion. Available color: black. Light and heat stabilized.Flexibility. High burst pressure and impact strength. Fit for use in a wi.. |
|||
Tensile Modulus | 0.640 GPa | 92.8 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® XE 4208 black 9992 PA612-I Product description: Grilamid XE 4208 black 9992 is a semiflexible high viscosity, plasticized, high impact and highly heat resistant polyamide 612 (PA612) extrusion grade. Unique properties of Gril.. |