Material Notes:
Product description: Grilamid XE 4208 black 9992 is a semiflexible high viscosity, plasticized, high impact and highly heat resistant polyamide 612 (PA612) extrusion grade. Unique properties of Grilamid XE 4208 black 9992 are: High strength, high burst pressure in tube formHigh heat resistanceSignificantly lower water absorption compared to standard polyamidesGood chemical and hydrolysis resistanceZincchloride resistanceLow densityEasy processing Application examples: Grilamid XE 4208 black 9992 was developed for media lines in passenger cars and trucks. Thanks to its excellent heat resistance it is particularly suitable for diesel, air brake, cooling, oil and hydraulic tubes. The product is not recommended for direct permanent contact with gasoline. One particular application is the use as outer layer of coextruded ECOSYS tubes. ECOSYS (EMS Cooling System) is the designation of multi-layered tubes developed by EMS-GRIVORY for automotive heating and cooling systems.Information provided by EMS Grivory
Physical Properties Metric English Comments
Density 1.03 g/cc
0.0372 lb/in³
ISO 1183
Water Absorption 2.0 %
2.0 %
ISO 62
Moisture Absorption 0.800 %
0.800 %
ISO 62
Mechanical Properties Metric English Comments
Ball Indentation Hardness 40.0 MPa
5800 psi
conditioned; ISO 2039-1
55.0 MPa
7980 psi
dry; ISO 2039-1
Tensile Stress 30.0 MPa

@Strain 50.0 %
4350 psi

@Strain 50.0 %
conditioned; ISO 527-1/-2
35.0 MPa

@Strain 50.0 %
5080 psi

@Strain 50.0 %
dry; ISO 527-1/-2
Elongation at Break >= 50 %
>= 50 %
dry; ISO 527-1/-2
>= 50 %
>= 50 %
conditioned; ISO 527-1/-2
Tensile Modulus 0.640 GPa
92.8 ksi
conditioned; ISO 527-1/-2
0.920 GPa
133 ksi
dry; ISO 527-1/-2
Charpy Impact Unnotched NB
NB
dry; ISO 179/1eU
NB
NB
conditioned; ISO 179/1eU
NB

@Temperature 30.0 °C
NB

@Temperature 86.0 °F
dry; ISO 179/1eU
NB

@Temperature 30.0 °C
NB

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Charpy Impact, Notched NB
NB
dry; ISO 179/1eA
NB
NB
conditioned; ISO 179/1eA
1.60 J/cm²

@Temperature 30.0 °C
7.61 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
1.60 J/cm²

@Temperature 30.0 °C
7.61 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 230 µm/m-°C
128 µin/in-°F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 130 µm/m-°C
72.2 µin/in-°F
ISO 11359-1/-2
Melting Point 213 °C
415 °F
10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 100 °C
212 °F
ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °C
122 °F
ISO 75-1/-2
Flammability, UL94 HB
HB
IEC 60695-11-10
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+10 ohm-cm
1.00e+10 ohm-cm
dry; IEC 60093
1.00e+10 ohm-cm
1.00e+10 ohm-cm
conditioned; IEC 60093
Surface Resistance 1.00e+10 ohm
1.00e+10 ohm
IEC 60093
Dielectric Strength 37.0 kV/mm
940 kV/in
dry; IEC 60243-1
37.0 kV/mm
940 kV/in
conditioned; IEC 60243-1
Comparative Tracking Index 600 V
600 V
conditioned; IEC 60112
Descriptive Properties Value Comments
Additives Plasticizer
Automotive Air intake sytems
Automotive electr. and electronics, lighting
Compressed air systems
Cooling and climate control
Hydraulic systems
Electricals & Electronics Cables & Tubes
Form Granules
Industry & Consumer goods Hydraulics & Pneumatics
Processing Other Extrusion
Profile Extrusion
Product Attributes High viscosity
Hydrolysis resistant
Special Characteristics High impact or impact modified
Improved heat resistance