Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 6.26 GPa | 908 ksi | ASTM D638 |
Plenco 50015 PET, Pellet, Injection Molded, White
(discontinued **) PLENCO 50015 is an engineering grade glass reinforced polyethylene terephthalate resin designed for increased flexibility and good physical strength. It is UL recognized and available in white, natu.. |
|||
Tensile Modulus | 6.26 GPa | 908 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL IGN320 PPE+PS 20% glass reinforced PPE + PS. High heat, high modulus automotive applications like ignition coils. |