Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 9.75 GPa | 1410 ksi | ISO 527-1/2 |
Radici Radilon® ARV300 (dry) Nylon 66 30% Glass-fiber reinforcedInformation provided by Radici group. |
|||
Tensile Modulus | 9.75 GPa | 1410 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® V4860HR PBT 30% glass reinforced PBT, UL94 V-0 rated, Hydrolytically stable, Impact Modified. |
|||
Tensile Modulus | 9.75 GPa | 1410 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Xenoy® 6370 PBT+PC 30% glass-reinforced, impact modified thermoplastic alloy. Improved toughness and ductility. |
|||
Tensile Modulus | 9.75 GPa | 1410 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® V4860HR PBT (Asia Pacific) 30% glass reinforced PBT, UL94 V-0 rated, Hydrolytically stable, Impact Modified. |
|||
Tensile Modulus | 9.75 GPa | 1410 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® V4860HR PBT (Europe-Africa-Middle East) 30% glass reinforced PBT, UL94 V-0 rated, Hydrolytically stable, Impact Modified. |