Radici Radilon® ARV300 (dry) Nylon 66

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 30% Glass Fiber Filled
Manufacturer Radici Group Plastics
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Radici Radilon® ARV300 (dry) Nylon 66.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
30% Glass-fiber reinforcedInformation provided by Radici group.
Physical Properties Metric English Comments
Specific Gravity 1.35 g/cc
1.35 g/cc
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength, Yield 180 MPa
26100 psi
ISO 527-1/2
Elongation at Break 3.7 %
3.7 %
ISO 527-1/2
Tensile Modulus 9.75 GPa
1410 ksi
ISO 527-1/2
Flexural Strength 260 MPa
37700 psi
ISO 178
Flexural Modulus 8.10 GPa
1170 ksi
ISO 178
Charpy Impact Unnotched 8.00 J/cm²
38.1 ft-lb/in²
ISO 179/1eU
Charpy Impact, Notched 1.40 J/cm²
6.66 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 260 °C
500 °F
ISO 1135 7-1-3
Deflection Temperature at 0.46 MPa (66 psi) 250 °C
482 °F
ISO 75/2Bf
Deflection Temperature at 1.8 MPa (264 psi) 235 °C
455 °F
ISO 75/2Af
Vicat Softening Point 245 °C
473 °F
ISO 306
Flammability, UL94 HB

@Thickness 0.800 mm
HB

@Thickness 0.0315 in