Polymer Property : Tensile Modulus = 9.57 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 9.57 GPa
1390 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP VERTON MX02795 PP
LNP* VERTON* MX02795 is a compound based on Polypropylene resin containing Proprietary Fillers. Added features of this material include: Heat Stabilized, UV Stabilized, Structural.
Tensile Modulus 9.57 GPa
1390 ksi
5 mm/min; ASTM D638
SABIC Innovative Plastics NORYL FE1630PW PPE+PS (Europe-Africa-Middle East)
Noryl* FE1630PW Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 30 % Glass Reinforced, injection moldable grade with improved hydrolytic stability; this grade has been developed for fluid en..