Polymer Property : Tensile Modulus = 9.05 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 9.05 GPa
1310 ksi
Radici Radiflam® A RV350AF (cond.) Nylon 66-35GF
PA66 flame retardant injection molding grade with red phosphorus, halogen free. 35% Glass fiber reinforced, for items with high stiffness and good dimensional stability.Information provided by Radic..
Tensile Modulus 9.05 GPa
1310 ksi
50 mm/min; ASTM D 638
SABIC Innovative Plastics LNP Thermocomp MF0069S PP
LNP* Thermocomp* MF0069S is a compound based on Polypropylene resin containing Glass Fiber, Flame Retardant. Added features of this material include: Chemically Coupled, Flame Retardant, Heat Stabi..