Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 9.02 GPa | 1310 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Thermocomp XF006S LNP* Thermocomp* XF006S is a compound based on Amorphous Nylon containing Glass Fiber. Characteristics of this grade are: Heat Stabilized.This data was supplied by SABIC-IP for the Americas region.. |
|||
Tensile Modulus | 9.02 GPa | 1310 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP XF006S PA LNP* THERMOCOMP* XF006S is a compound based on Amorphous Nylon containing 30% Glass Fiber. Added feature of th is grade is: Heat Stabilized. |