Polymer Property : Tensile Modulus = 898 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 6.19 GPa
898 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRICOMP WFL33 PBT
LNP* LUBRICOMP* WFL33 is a compound based on PBT containing 15% Glass Fiber, 15% PTFE. Added feature of this grade is: Wear Resistant.
Tensile Modulus 6.19 GPa
898 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP DF004P PC
LNP THERMOCOMP* DF004P is a compound based on Polycarbonate resin containing 20% Glass Fiber. Added features of this material include: Exceptional Processing.
Tensile Modulus 6.19 GPa
898 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP 2F005 ETFE
LNP* Thermocomp* 2F005 is a fluoropolymer compound based on ETFE containing 25% Glass Fiber.