Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.618 GPa | 89.6 ksi | 1% Secant; ASTM D 638 |
NOVA Chemicals Surpass® IFs730-R Octene sMDPE Food Packaging Lid Resin IFs730-R complies with the U.S. FDA regulations for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food.NOVA Chem.. |