Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

NOVA Chemicals Surpass® IFs730-R Octene sMDPE Food Packaging Lid Resin

Category Polymer , Thermoplastic , Polyethylene (PE) , MDPE , Medium Density Polyethylene (MDPE), Molded
Manufacturer NOVA Chemicals
Trade Name Surpass®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NOVA Chemicals Surpass® IFs730-R Octene sMDPE Food Packaging Lid Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
IFs730-R complies with the U.S. FDA regulations for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food.NOVA Chemicals' polyethylene resins are biologically and chemically inert.Features: Outstanding processability yielding improved cycle times, Low warpage for improved part quality and reliability, Superior cold temperature impact resistance, Excellent organoleptic propertiesAdditives: Antioxidant, Mold releaseApplications: Thin wall lids for food packaging containers
Physical Properties Metric English Comments
Density 0.930 g/cc
0.0336 lb/in³
ASTM D 792
Melt Flow 85 g/10 min

@Load 2.16 kg,
Temperature 190 °C
85 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D 1238
Mechanical Properties Metric English Comments
Hardness, Shore D 62
62
ASTM D 2240
Tensile Strength at Break 9.20 MPa
1330 psi
Rate of 50 mm/min; ASTM D 638
Tensile Strength, Yield 15.2 MPa
2200 psi
Rate of 50 mm/min; ASTM D 638
Elongation at Break 104 %
104 %
Rate of 50 mm/min; ASTM D 638
Elongation at Yield 12 %
12 %
Rate of 50 mm/min; ASTM D 638
Tensile Modulus 0.618 GPa
89.6 ksi
1% Secant; ASTM D 638
Flexural Modulus, 1% Secant 526 MPa
76300 psi
ASTM D 790
Thermal Properties Metric English Comments
Vicat Softening Point 101 °C
214 °F
ASTM 1525