Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 5.86 GPa | 850 ksi | ASTM D638 |
Oxford Polymers 10GF 10% Glass Fiber Filled Polyetherimide for Extrusion and Injection Molding 10% Glass Fiber Filled Polyetherimide for Extrusion and Injection MoldingInformation provided by Oxford Polymers. |
|||
Tensile Modulus | 5.86 GPa @Temperature 22.8 °C |
850 ksi @Temperature 73.0 °F |
ASTM D638 |
Quadrant EPP Ketron® HPV PEEK High Pressure Velocity Polyetherether Ketone (ASTM Product Data Sheet) This bearing grade of extruded Ketron PEEK offers the lowest coefficient of friction and best machinability of all Ketron grades. It is ideal for low wear, high PV parts that require chemical resis.. |
|||
Tensile Modulus | 5.86 GPa | 850 ksi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Edgetek® PS-15GF/000 FR Polybutylene Terephthalate (PBT), Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedIgnition ResistantUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Tensile Modulus | 5.86 GPa | 850 ksi | ASTM D638 |
Quadrant EPP Duratron® PBI CU60 Polybenzimidazole, unfilled, compression molded (ASTM Product Data Sheet) Duratron® PBI is the highest performance engineering plastic available from Quadrant EPP. It offers the highest mechanical properties of any thermoplastic above 400° F (205° C). Duratron® PBI .. |
|||
Tensile Modulus | 5.86 GPa | 850 ksi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Edgetek® AS-20CF/000 Acrylonitrile Butadiene Styrene (ABS), Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Tensile Modulus | 5.86 GPa | 850 ksi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Stat-Tech™ AS-15NCF/000 ABS - 15% Nickel Coated Carbon Fiber
(discontinued **) Data provided by PolyOne. |
|||
Tensile Modulus | 5.86 GPa | 850 ksi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Edgetek® NL-08GF-02CF/000 Nylon 6/12, Glass/Carbon Fiber Filled
(discontinued **) Description/Features:Glass/Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Tensile Modulus | 5.86 GPa | 850 ksi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Lubri-Tech™ NL-15CF-15GF/5M Nylon 6/12, Carbon/Glass Filled
(discontinued **) Description/Features:Carbon Fiber ReinforcedGlass Fiber ReinforcedMolybdenum Disulfide LubricatedInformation provided by PolyOne Corporation. |
|||
Tensile Modulus | 5.86 GPa | 850 ksi | ASTM D638 |
Fiberfil® J-60/30 Polypropylene Homopolymer, 30% Glass Reinforced Information provided by FIBERFIL Engineered Plastics |
|||
Tensile Modulus | 5.86 GPa | 850 ksi | ASTM D638 |
Fiberfil® J-60/30/E/HF Polypropylene Homopolymer, 30% Glass Reinforced, Chemically coupled, improved flow Information provided by FIBERFIL Engineered Plastics |
|||
Tensile Modulus | 5.86 GPa | 850 ksi | ASTM D638 |
Fiberfil® J-60/30/E8 Polypropylene Homopolymer, 30% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Tensile Modulus | 5.86 GPa | 850 ksi | ASTM D638 |
Star Plastics ABSGF30 Molding Grade ABS With 30% Glass Information provided by Star Plastics, Inc. |
|||
Tensile Modulus | 5.86 GPa | 850 ksi | ASTM D638 |
Ensinger Tecapeek® XP-96BHT Compression Molded PEEK HT, Unfilled, Black Pigmented Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in.. |
|||
Tensile Modulus | 5.86 GPa | 850 ksi | ASTM Test |
BASF Ultramid® A3EG3 15% Glass Filled PA66 (Dry) Ultramid A3EG3 is a 15% glass fiber reinforced injection molding PA66 grade. It conforms to FDA requirements of 21 CFR 177.1500. |
|||
Tensile Modulus | 5.86 GPa | 850 ksi | ASTM D638 |
Fiberfil® J-60/30/E5 Polypropylene Homopolymer, 30% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |