Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 8.85 GPa | 1280 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP RFN14 PA 66 LNP* LUBRICOMP* RFN14 is a compound based on Nylon 66 containing 20% Glass Fiber, 5% MOS2. Added features of this grade include: Wear Resistant. |