Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.0593 GPa | 8.60 ksi | Molded Properties; ISO 527-2 |
ExxonMobil Escorene™ UL 00514 Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: UL 00514 is a copolymer of ethylene and vinyl acetate.Processing Conditions: Processing temperatures above 250°C (482°F) may cause resin degradation.Availability: Africa & Mid.. |