Polymer Property : Tensile Modulus = 0.0593 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 0.0593 GPa
8.60 ksi
Molded Properties; ISO 527-2
ExxonMobil Escorene™ UL 00514 Ethylene Vinyl Acetate Copolymer (European Grade)
Product Description: UL 00514 is a copolymer of ethylene and vinyl acetate.Processing Conditions: Processing temperatures above 250°C (482°F) may cause resin degradation.Availability: Africa & Mid..