Mechanical Properties Metric English Comments
Tensile Modulus 5.499 GPa
797.6 ksi
DIN EN ISO 527
Wolf Kunststoff ZEDEX® ZX-410V7T A4T Polymer Alloy, Fiber Reinforced, Friction Modified
Main Characteristics: Fiber-reinforced; Friction-modified; Very high stiffness (higher than that of fiber-reinforced PEEK); Very low thermal expansion coefficient; Low friction; High wear resistance..
Tensile Modulus 5.499 GPa
797.6 ksi
ASTM D638
Aclo Accutech Polycarbonate POL050G40L Glass Reinforced
Copyright © lookpolymers.com All Rights Reserved