Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 5.499 GPa | 797.6 ksi | DIN EN ISO 527 |
Wolf Kunststoff ZEDEX® ZX-410V7T A4T Polymer Alloy, Fiber Reinforced, Friction Modified Main Characteristics: Fiber-reinforced; Friction-modified; Very high stiffness (higher than that of fiber-reinforced PEEK); Very low thermal expansion coefficient; Low friction; High wear resistance.. |
|||
Tensile Modulus | 5.499 GPa | 797.6 ksi | ASTM D638 |
Aclo Accutech Polycarbonate POL050G40L Glass Reinforced |