Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.545 GPa | 79.0 ksi | 1 mm/min |
Arkema Group Rilsan® AMN P30 LD Nylon 12, Flexible, Injection Grade (Conditioned) Designation ISO 1874-PA12-P,MLR,12-004Flexible grade for injection molding. Available color: black. Light stabilized. Mold-release agent.Good impact strength. Flexibility and dynamic properties. Eas.. |