Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 4.96 GPa | 719 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Thermocomp DFZ22E PC LNP* Thermocomp* DFZ22E is a compound based on Polycarbonate with Glass and Milled Fiber. Characteristics of this products is Easy Molding.This data was supplied by SABIC-IP for the Americas region.. |
|||
Tensile Modulus | 4.96 GPa | 719 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP RW004 PA 66 (Asia Pacific) LNP* THERMOCOMP* RW004 is a compound based on Nylon 66 resin containing Mineral. |
|||
Tensile Modulus | 4.96 GPa | 719 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP RW004 PA 66 LNP THERMOCOMP* RW004 is a compound based on Nylon 66 resin containing Wollastonite. |