Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 48.3 GPa | 7010 ksi | ASTM D638 |
Quantum Composites HTC-9590 55% Carbon Fiber Reinforced Bismaleimide SMC, High Temperature Composite HTC-9590 (127-51-3) is a 12K Pan Based Carbon Fiber reinforced Bismaleimide (BMI) ESC (Engineered Structural Composite) molding compound. It exhibits outstanding elevated temperature characteristic.. |