Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 7.49 GPa | 1090 ksi | 1mm/min; ISO 527 |
BASF Ultramid® 8234G HS 44% Glass Filled PA6 (Conditioned) Ultramid 8234G HS is a heat stabilized, 44% glass fiber reinforced polyamide 6 injection molding compound offering the highest level of strength, stiffness, high temperature performance and dimensio.. |
|||
Tensile Modulus | 7.49 GPa | 1090 ksi | same value from ASTM and ISO test. |
BASF Capron® 8234G 44% Glass-Filled Nylon 6 (Conditioned)
(discontinued **) Capron 8234G is a 44% glass fiber reinforced polyamide 6 injection molding compound offering the highest level of strength, stiffness, high temperature performance and dimensional stability. It is .. |
|||
Tensile Modulus | 7.49 GPa | 1090 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP PFB91S PA 6 LNP* THERMOCOMP* PFB91S is a compound based on Nylon 6 resin containing Proprietary Filler(s). |