Polymer Property : Tensile Modulus = 687 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 4.74 GPa
687 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP STAT-LOY PF303 PA 6
LNP* STAT-LOY* PF303 is a Nylon 6 base resin containing 15% Glass Fiber. Added features of this grade includes: Antistat.
Tensile Modulus 4.74 GPa
687 ksi
ASTM Data
Dow Retain® 8209 ABS + Polycarbonate
Data provided by Dow Chemical.