Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 4.65 GPa | 675 ksi | ASTM D638 |
Quadrant EPP Nylatron® GF30 Nylon Type 66, 30% Glass-Reinforced Black Color (ASTM Product Data Sheet) |
|||
Tensile Modulus | 4.65 GPa | 675 ksi | ASTM D638 |
Fiberfil® M-1812 Polypropylene Homopolymer, 45% Talc Filled Information provided by FIBERFIL Engineered Plastics |
|||
Tensile Modulus | 4.65 GPa | 675 ksi | ASTM D638 |
Ensinger DELRIN® 570 Acetal, 20% Glass Filled (POM) DELRIN®570 Shapes manufactured by Ensinger are 20% glass filled materials intended for general industrial use. The material offers very high stiffness, low warpage, and low creep for superior part .. |