Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.441 GPa | 64.0 ksi | ASTM D4894 |
Saint-Gobain Fluoroloy® A15 High Performance Seal Material Improved sealing at low pressure; Can be abrasive running against soft metals
Information provided by Saint-Gobain Performance Plastics. |